Hony Engineering Plastics Limited
Hony Engineering Plastics Limited
Home> Industry Information> German Rochling Gray Durostone CFR767

German Rochling Gray Durostone CFR767

May 18, 2023

German Rochling Gray durostone CFR767


CFR767-3


The combination of processing cycles in high temperature environments combined with aggressive fluxes can cause degradation of standard Durostone grades.

The solution is Durostone CFR767, which is specially formulated for aggressive fluxes and high temperature process configurations.

The resin used to produce Durostone CFR767 can withstand temperatures up to 300°C. When the solder bath temperature exceeds 265°C and the bottom PCB preheat exceeds 140°C, Durostone CFR767 should be used instead of the standard grade.

Durostone CFR767 has excellent flux resistance. When fluxes containing halides or dicarboxylic acids are used in high-volume production, the lifetime of standard grade materials is reduced, so Durostone CFR767 is the ideal solution.

The above is the German Rochling Gray Durostone CFR767 we have listed for you. You can submit the following form to obtain more industry information we provide for you.

You can visit our website or contact us, and we will provide the latest consultation and solutions

Share to:

Send Inquiry

Home> Industry Information> German Rochling Gray Durostone CFR767
We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Send